Aerogel waterproof and heat-insulating roll

Product modelunitsParametersTesting standards / methods
Length (Negative deviations are not allowed)min20 Measuring tape
Width (allowable deviation ±10mm)/1000 Measuring tape
Thickness (allowable deviation ±0.15mm)
1.5、2.0Thickness gauge
Having viscosityN/mm≥ 25JC/T 942-2004
Heat resistance/No flowing, cracking, or deformation
Softness and gentleness/No cracks
Peel strength (color steel sheet)/≥ 0.8
Solar light reflection ratio/0.82 JG/T 235-2014
Thermal insulation temperature difference (1.5mm)≥ 25HG/T 4341-2012
Thermal insulation temperature difference (2mm)≥ 33