Heat-temperature coating

Product SpecificationsunitsAG-T200AG-T400AG-T600                       
Packaging/10kg/20L
Appearance/Greyish viscous paste
Construction method/Scraping, applying, spraying
Thermal conductivity at normal temperatureW/(m ·K)0.035~0.0400.035~0.0400.065~0.080
Dry densityKg/m³300~400400~500800~900
Square meter usage (1mm thick)Kg/m²1.5 
Operating temperature150 ≤ 450≤ 650
Construction temperature

Operation at temperatures

 below 150℃

5~955~95
Flame resistance performanceGradeFlame retardantFlame retardantFlame retardant
Bonding strengthMpa≥0.6≥0.4≥0.15
Drying timeh2mm coating:

At room temperature, the surface drying time is ≤ 16 hours, and the full drying time 

is ≤ 48 hours

Coating service life

The construction must be carried out strictly in accordance with the construction plan 

and the usage amount of construction materials.

During the warranty period, the coating surface shall not crack or fall off. The warranty period is 8 to 10 years.